<?xml version="1.0" encoding="UTF-8"?><xml><records><record><source-app name="Biblio" version="7.x">Drupal-Biblio</source-app><ref-type>17</ref-type><contributors><authors><author><style face="normal" font="default" size="100%">Devassy, Biju M.</style></author><author><style face="normal" font="default" size="100%">Shanbhag, G. V.</style></author><author><style face="normal" font="default" size="100%">Mirajkar, Subhash P.</style></author><author><style face="normal" font="default" size="100%">Bohringer, Walter</style></author><author><style face="normal" font="default" size="100%">Fletcher, Jack C. Q.</style></author><author><style face="normal" font="default" size="100%">Halligudi, Shivaraj B.</style></author></authors></contributors><titles><title><style face="normal" font="default" size="100%">Silicotungstate-modified zirconia as an efficient catalyst for phenol tert-butylation</style></title><secondary-title><style face="normal" font="default" size="100%">Journal of Molecular Catalysis A-Chemical</style></secondary-title></titles><keywords><keyword><style  face="normal" font="default" size="100%">phenol</style></keyword><keyword><style  face="normal" font="default" size="100%">Silicotungstic acid</style></keyword><keyword><style  face="normal" font="default" size="100%">tert-butylation</style></keyword><keyword><style  face="normal" font="default" size="100%">Zirconia</style></keyword></keywords><dates><year><style  face="normal" font="default" size="100%">2005</style></year><pub-dates><date><style  face="normal" font="default" size="100%">MAY</style></date></pub-dates></dates><number><style face="normal" font="default" size="100%">1-2</style></number><publisher><style face="normal" font="default" size="100%">ELSEVIER SCIENCE BV</style></publisher><pub-location><style face="normal" font="default" size="100%">PO BOX 211, 1000 AE AMSTERDAM, NETHERLANDS</style></pub-location><volume><style face="normal" font="default" size="100%">233</style></volume><pages><style face="normal" font="default" size="100%">141-146</style></pages><language><style face="normal" font="default" size="100%">eng</style></language><abstract><style face="normal" font="default" size="100%">&lt;p&gt;The alkylation of phenol with tert-butanol was investigated using zirconia modified with silicotungstic acid (STA) as catalysts. The catalysts with different STA loading (5-25 wt.% calcined at 750 degrees C) and calcination temperature (15 wt.% calcined from 350 to 850 degrees C) were prepared and characterized by X-ray diffraction and NH3-TPD measurements. The XRD results indicate that STA stabilizes the tetragonal phase of zirconia. The catalyst with 15% STA on ZrO2 calcined at 750 degrees C shows the highest acidity and hence highest activity. Under the reaction conditions of 140 degrees C, tert-butanol/phenol molar ratio of 2 and LHSV of 4 h(-1), phenol conversion was 95.4% with selectivity to 2-tert-butyl phenol 4.3%, 4-tert-butyl phenol 59.2% and 2,4-di-tert-butyl phenol 35.8%. The reaction was studied as a function of time for 50 It without appreciable change in phenol conversion and product selectivity. The deactivated catalyst could be regenerated by calcination with out appreciable lose in catalytic activity and product selectivity. (c) 2005 Elsevier B.V. All rights reserved.&lt;/p&gt;</style></abstract><issue><style face="normal" font="default" size="100%">1-2</style></issue><work-type><style face="normal" font="default" size="100%">Article</style></work-type><custom3><style face="normal" font="default" size="100%">Foreign</style></custom3><custom4><style face="normal" font="default" size="100%">3.958</style></custom4></record><record><source-app name="Biblio" version="7.x">Drupal-Biblio</source-app><ref-type>17</ref-type><contributors><authors><author><style face="normal" font="default" size="100%">Sarish, S.</style></author><author><style face="normal" font="default" size="100%">Devassy, Biju M.</style></author><author><style face="normal" font="default" size="100%">Halligudi, Shivaraj B.</style></author></authors></contributors><titles><title><style face="normal" font="default" size="100%">tert-Butylation of p-cresol over WOx/ZrO2 solid acid catalysts</style></title><secondary-title><style face="normal" font="default" size="100%">Journal of Molecular Catalysis A - Chemical</style></secondary-title></titles><keywords><keyword><style  face="normal" font="default" size="100%">p-Cresol</style></keyword><keyword><style  face="normal" font="default" size="100%">tert-butylation</style></keyword><keyword><style  face="normal" font="default" size="100%">tungsten oxide</style></keyword><keyword><style  face="normal" font="default" size="100%">Zirconia</style></keyword></keywords><dates><year><style  face="normal" font="default" size="100%">2005</style></year><pub-dates><date><style  face="normal" font="default" size="100%">JUL</style></date></pub-dates></dates><number><style face="normal" font="default" size="100%">1-2</style></number><publisher><style face="normal" font="default" size="100%">ELSEVIER SCIENCE BV</style></publisher><pub-location><style face="normal" font="default" size="100%">PO BOX 211, 1000 AE AMSTERDAM, NETHERLANDS</style></pub-location><volume><style face="normal" font="default" size="100%">235</style></volume><pages><style face="normal" font="default" size="100%">44-51</style></pages><language><style face="normal" font="default" size="100%">eng</style></language><abstract><style face="normal" font="default" size="100%">&lt;p&gt;The tert-butylation of p-cresol with tert-butanol was carried out over WO3/ZrO2 catalysts under flow conditions, The catalysts were prepared by wet impregnation method using zirconium oxyhydroxide and ammonium metatungstate. Catalysts with different WO3 loading (5-30 wt.%) were prepared and calcined at 800 degrees C and catalyst with 15% WO,, was calcined from 600 to 900 C. The catalysts were characterized by surface area, XRD, FTIR and TEM. The catalyst 15% WO3/ZrO2 calcined at 800 degrees C found to be the most active in the reaction. The effect of temperature, space velocity and molar ratio of the reactants on the conversion of p-cresol and products selectivities were studied. Under the optimized reaction conditions of 130 degrees C, tert-butanol/p-cresol molar ratio of 3 and flow rate of 10 ml h(-1). p-cresol conversion was 69.8% with selectivity to 2-tert-butyl-p-cresol 92.4%, 2,6-di-tert-butyl-p-cresol 6.3% and p-cresol tert-butyl ether 1.3%. The catalytic activity is compared with sulfated zirconia, USY, H beta zeolites and montmorillonite K-10 under the optimized reaction conditions The activity of sulfated zirconia is lower than that of 15% WO3/ZrO2 catalyst calcined at 800 C and other catalysts showed very low activity, (c) 2005 Elsevier B.V.. All rights reserved.&lt;/p&gt;</style></abstract><issue><style face="normal" font="default" size="100%">1-2</style></issue><work-type><style face="normal" font="default" size="100%">Article</style></work-type><custom3><style face="normal" font="default" size="100%">&lt;p&gt;Foreign&lt;/p&gt;</style></custom3><custom4><style face="normal" font="default" size="100%">3.958</style></custom4></record><record><source-app name="Biblio" version="7.x">Drupal-Biblio</source-app><ref-type>17</ref-type><contributors><authors><author><style face="normal" font="default" size="100%">Devassy, Biju M.</style></author><author><style face="normal" font="default" size="100%">Shanbhag, G.V.</style></author><author><style face="normal" font="default" size="100%">Halligudi,  S.B.</style></author></authors></contributors><titles><title><style face="normal" font="default" size="100%">Phenol tert-butylation over zirconia-supported 12-molybdophosphoric acid catalyst</style></title><secondary-title><style face="normal" font="default" size="100%">Journal of Molecular Catalysis A-Chemical</style></secondary-title></titles><keywords><keyword><style  face="normal" font="default" size="100%">12-molybdophosphoric acid</style></keyword><keyword><style  face="normal" font="default" size="100%">phenol</style></keyword><keyword><style  face="normal" font="default" size="100%">tert-butylation</style></keyword><keyword><style  face="normal" font="default" size="100%">Zirconia</style></keyword></keywords><dates><year><style  face="normal" font="default" size="100%">2006</style></year><pub-dates><date><style  face="normal" font="default" size="100%">MAR</style></date></pub-dates></dates><number><style face="normal" font="default" size="100%">1-2</style></number><publisher><style face="normal" font="default" size="100%">ELSEVIER SCIENCE BV</style></publisher><pub-location><style face="normal" font="default" size="100%">PO BOX 211, 1000 AE AMSTERDAM, NETHERLANDS</style></pub-location><volume><style face="normal" font="default" size="100%">247</style></volume><pages><style face="normal" font="default" size="100%">162-170</style></pages><language><style face="normal" font="default" size="100%">eng</style></language><abstract><style face="normal" font="default" size="100%">&lt;p&gt;The alkylation of phenol with tert-butanol was investigated using zirconia-supported 12-molybdophosphoric acid (MPA) as catalyst. The catalysts with different MPA loading (5-25 wt.% calcined at 700 degrees C) and calcination temperature (15 wt.% calcined from 500 to 750 degrees C) were prepared by suspending zirconium oxyhydroxide in methanol solution of MPA followed by drying and calcination. These catalysts were characterized by X-ray diffraction and (31)p MAS NMR spectroscopy measurements. The XRD results indicated that MPA stabilizes the tetragonal phase of zirconia. (31)p MAS NMR spectra showed the presence of three types of phosphorous species, phosphomolybdate in interaction with zirconia, decomposition product of MFPA and an unidentified species. IFTIR pyridine adsorption on 15% MPA catalyst calcined at different temperatures showed the presence of both Bronsted and Lewis acidity and the catalyst calcined at 700 degrees C showed the highest relative Bronsted acidity. Under the reaction conditions of 140 degrees C, tert-butanol/phenol molar ratio of 2 and LHSV of 4 h(-1), the phenol conversion was 80.6% at 2 h (selectivity to 2-TBP 11.5%, 2,4-DTBP 55.2%, and 4-TBP 25.7%), which decreased slowly with time and at 31 h, it was 58.5% (selectivity to 2-TBP 15.2%, 2,4-DTBP 41.6%, and 4-TBP 38.4%). The major reason for the catalyst deactivation was the reduction and leaching of MPA from the catalyst surface. (c) 2005 Elsevier B.V. All rights reserved.&lt;/p&gt;</style></abstract><issue><style face="normal" font="default" size="100%">1-2</style></issue><work-type><style face="normal" font="default" size="100%">Article</style></work-type><custom3><style face="normal" font="default" size="100%">&lt;p&gt;Foreign&lt;/p&gt;</style></custom3><custom4><style face="normal" font="default" size="100%">3.958</style></custom4></record></records></xml>