<?xml version="1.0" encoding="UTF-8"?><xml><records><record><source-app name="Biblio" version="7.x">Drupal-Biblio</source-app><ref-type>17</ref-type><contributors><authors><author><style face="normal" font="default" size="100%">Anantharamaiah, P. N.</style></author><author><style face="normal" font="default" size="100%">Joy, P. A.</style></author></authors></contributors><titles><title><style face="normal" font="default" size="100%">High magnetostriction parameters of sintered and magnetic field annealed Ga-substituted CoFe2O4</style></title><secondary-title><style face="normal" font="default" size="100%">Materials Letters</style></secondary-title></titles><keywords><keyword><style  face="normal" font="default" size="100%">Cobalt ferrite</style></keyword><keyword><style  face="normal" font="default" size="100%">Magnetic field annealing</style></keyword><keyword><style  face="normal" font="default" size="100%">Magnetic materials</style></keyword><keyword><style  face="normal" font="default" size="100%">Magnetostriction</style></keyword><keyword><style  face="normal" font="default" size="100%">Substitution</style></keyword></keywords><dates><year><style  face="normal" font="default" size="100%">2017</style></year><pub-dates><date><style  face="normal" font="default" size="100%">APR </style></date></pub-dates></dates><volume><style face="normal" font="default" size="100%">192</style></volume><pages><style face="normal" font="default" size="100%">169-172</style></pages><language><style face="normal" font="default" size="100%">eng</style></language><abstract><style face="normal" font="default" size="100%">&lt;p&gt;Impact of substitution of the non-magnetic ion Ga3+ for Fe3+ on the magnetostriction parameters of CoFe2O4 has been investigated for samples prepared by a tartrate-gel method. All the Ga-substituted compositions in CoGaxFe2-xO4 (0 &amp;lt;= x &amp;lt;= 0.3) showed higher strain sensitivity (d lambda/dH), at low magnetic fields, compared to that of the unsubstituted sample. The magnetostriction strain (lambda) and d lambda/dH of the composition CoGa0.1Fe1.9O4 could be enhanced from -228 to -296 ppm and -2.20 x 10(-9) to -3.55 x 10(-9) miA, respectively, at low magnetic fields, after magnetic field annealing at 300 degrees C. (C) 2016 Elsevier B.V. All rights reserved.&lt;/p&gt;</style></abstract><work-type><style face="normal" font="default" size="100%">Article</style></work-type><custom3><style face="normal" font="default" size="100%">Foreign</style></custom3><custom4><style face="normal" font="default" size="100%">2.687</style></custom4></record></records></xml>