<?xml version="1.0" encoding="UTF-8"?><xml><records><record><source-app name="Biblio" version="7.x">Drupal-Biblio</source-app><ref-type>17</ref-type><contributors><authors><author><style face="normal" font="default" size="100%">Gaikwad, S. P.</style></author><author><style face="normal" font="default" size="100%">Dhage, S. R.</style></author><author><style face="normal" font="default" size="100%">Potdar, H. S.</style></author><author><style face="normal" font="default" size="100%">Samuel, V.</style></author><author><style face="normal" font="default" size="100%">Ravi, V.</style></author></authors></contributors><titles><title><style face="normal" font="default" size="100%">Co-precipitation method for the preparation of nanocrystalline ferroelectric SrBi2Nb2O9 ceramics</style></title><secondary-title><style face="normal" font="default" size="100%">Journal of Electroceramics</style></secondary-title></titles><keywords><keyword><style  face="normal" font="default" size="100%">Ceramics</style></keyword><keyword><style  face="normal" font="default" size="100%">Chemical synthesis</style></keyword><keyword><style  face="normal" font="default" size="100%">electronic materials</style></keyword><keyword><style  face="normal" font="default" size="100%">ferroelectricity</style></keyword><keyword><style  face="normal" font="default" size="100%">Oxides</style></keyword></keywords><dates><year><style  face="normal" font="default" size="100%">2005</style></year><pub-dates><date><style  face="normal" font="default" size="100%">JAN</style></date></pub-dates></dates><number><style face="normal" font="default" size="100%">1</style></number><publisher><style face="normal" font="default" size="100%">SPRINGER</style></publisher><pub-location><style face="normal" font="default" size="100%">VAN GODEWIJCKSTRAAT 30, 3311 GZ DORDRECHT, NETHERLANDS</style></pub-location><volume><style face="normal" font="default" size="100%">14</style></volume><pages><style face="normal" font="default" size="100%">83-87</style></pages><language><style face="normal" font="default" size="100%">eng</style></language><abstract><style face="normal" font="default" size="100%">&lt;p&gt;A simple co-precipitation technique had been successfully applied for the preparation of pure ultrafine single phase SrBi2Nb2O9. Ammonium hydroxide and ammonium oxalate were used to precipitate Sr2+, Bi3+ and Nb5+ cations simultaneously. No pyrochlore phase was found while heating powder at 850 C and pure SrBi2Nb2O9 (SBN) phase was formed as revealed by the X-ray diffraction (XRD) studies. Particle size and morphology was studied by transmission electron microscopy (TEM). The room temperature dielectric constant at 1 kHz is 100. The ferroelectric hysteresis loop parameters of these samples were also studied.&lt;/p&gt;</style></abstract><issue><style face="normal" font="default" size="100%">1</style></issue><work-type><style face="normal" font="default" size="100%">Article</style></work-type><custom3><style face="normal" font="default" size="100%">&lt;p&gt;Foreign&lt;/p&gt;</style></custom3><custom4><style face="normal" font="default" size="100%">1.263</style></custom4></record><record><source-app name="Biblio" version="7.x">Drupal-Biblio</source-app><ref-type>17</ref-type><contributors><authors><author><style face="normal" font="default" size="100%">Murugan, A. Vadivel</style></author><author><style face="normal" font="default" size="100%">Gaikwad, A. B.</style></author><author><style face="normal" font="default" size="100%">Samuel, V.</style></author><author><style face="normal" font="default" size="100%">Ravi, V.</style></author></authors></contributors><titles><title><style face="normal" font="default" size="100%">Coprecipitation technique to prepare Sr0.5Ba0.5Nb2O6</style></title><secondary-title><style face="normal" font="default" size="100%">Bulletin of Materials Science</style></secondary-title></titles><keywords><keyword><style  face="normal" font="default" size="100%">Ceramics</style></keyword><keyword><style  face="normal" font="default" size="100%">Electron microscopy</style></keyword><keyword><style  face="normal" font="default" size="100%">ferroelectricity</style></keyword><keyword><style  face="normal" font="default" size="100%">Oxides</style></keyword><keyword><style  face="normal" font="default" size="100%">X-ray diffraction</style></keyword></keywords><dates><year><style  face="normal" font="default" size="100%">2006</style></year><pub-dates><date><style  face="normal" font="default" size="100%">JUN</style></date></pub-dates></dates><number><style face="normal" font="default" size="100%">3</style></number><publisher><style face="normal" font="default" size="100%">INDIAN ACADEMY SCIENCES</style></publisher><pub-location><style face="normal" font="default" size="100%">C V RAMAN AVENUE, SADASHIVANAGAR, P B \#8005, BANGALORE 560 080, INDIA</style></pub-location><volume><style face="normal" font="default" size="100%">29</style></volume><pages><style face="normal" font="default" size="100%">221-223</style></pages><language><style face="normal" font="default" size="100%">eng</style></language><abstract><style face="normal" font="default" size="100%">&lt;p&gt;An aqueous mixture of ammonium oxalate and ammonium hydroxide was used to coprecipitate barium and strontium ions as oxalates and niobium ions as hydroxide under basic conditions. This precursor on calcining at 750 degrees C yielded Sr0.5Ba0.5Nb2O6 phase. This is a much lower temperature than that prepared by traditional solid state method (1000 degrees C) as reported for the formation of Sr0.5Ba0.5Nb2O6 (SBN). Transmission electron microscopic (TEM) investigations revealed that the average particle size was 80 nm for the calcined powders. The room temperature dielectric constant at I kHz was found to be 1100. The ferroelectric hysteresis loop parameters of these samples were also studied.&lt;/p&gt;</style></abstract><issue><style face="normal" font="default" size="100%">3</style></issue><work-type><style face="normal" font="default" size="100%">Article</style></work-type><custom3><style face="normal" font="default" size="100%">&lt;p&gt;Indian&lt;/p&gt;</style></custom3><custom4><style face="normal" font="default" size="100%">0.895</style></custom4></record></records></xml>